Ultrasonic Examination of Butt-welds in Plates
Butt-welds in all tank wall courses subjected to a maximum actual operating membrane tensile stress, perpendicular to the welded joint, greater than 0.1 times the specified minimum tensile strength of the API620 large vertical storage tanks foundations plate material shall be completely examined.
Butt-welds in API 620 oil tank wall courses subjected to maximum actual operating membrane tensile stress, perpendicular to the welded joint, less than or equal to 0.1 times the specified minimum tensile strength of plate material shall be spot examined in accordance with Figure Q-2.

The after-sales service personnel understand the user's ideas and needs in detail, and stand on the other side's position and interests. Actively communicate with users and help them solve practical problems. This not only solves the service problem, but also improves the customer's trust in the company.

The annual sales volume of steel product is over 300,000 tons, and the sales volume has increased year by year. The business scope covers the Southeast Asia, Eastern Europe, Middle East, Africa, North America, and South America. Client services are mainly in the petrochemical, wind power, shipbuilding, steel structure, machinery manufacturing, and construction industries. Throughout the process, we provide customers with professional personal steel customization services and one-stop solutions, professionally set a variety of futures, fast delivery, and excellent prices.

Weld inspection of API620 large vertical storage tanks foundations, vertical oil tank wall plate: In the welding inspection process of oil tank wall plate, attention should be paid to the defects of thick wall plate, such as incomplete penetration, incomplete root fusion and cracks. If there is a root incomplete penetration defect, it is necessary to open the weld joint with carbon arc air gouging and grinding machine grinding, or even weld through, and then weld again after the defect is removed.

Previous : API 620 welded steel flat-bottom tanks roof load

Next : API 620 cylindrical oil storage tanks material ASTM A516

Leave a message

Client Image 1
Client Image 2
Client Image 3
Client Image 4
Client Image 5
Client Image 6
Client Image 7
Client Image 8
Client Image 9
Client Image 10
Client Image 11
Client Image 12